Epoxy Zinc-Rich Primer

Coating Application of Zinc Rich Epoxy Paint
Mixing mass ratio: Base material (A): The curing agent (B) = 10: 1.
Theoretical amount: 220 g / m2.
Painting passes: spraying or brushing 2 to 3, 60 to 80 microns dry.
Mixing: Use a power mixer component A (base) Stir, then stirring state by mixing ratio of the added amount of group B (curing agent), and fully mixed, while stirring continued momentum needed painting.
Thinner or Cleaner: For supporting diluent.
Curing time: After mixed directly.